CVR 3 is a natural mortar based on natural hydraulic lime designed to carry out restoration work for historic buildings.
The figure below reports the shear viscosity as a function of shear rate for sample CVR 3. The viscosity ranged from 4300 to 1 Pa·s for a shear rate variation from 0.1 to 100 s-1. The reported values indicate a mortar with good workability.
The picture below shows the diffractino spectrography of material CVR3.
Ist historischer Werkstoff: | true |